Aluminium Alloy // Commercial Alloy // 6026 - T9

Chemical Element % Present
Manganese (Mn) 0.20 - 1.00
Iron (Fe) 0.0 - 0.70
Magnesium (Mg) 0.60 - 1.20
Silicon (Si) 0.60 - 1.40
Copper (Cu) 0.20 - 0.50
Lead (Pb) 0.0 - 0.40
Bismuth (Bi) 0.50 - 1.50
Zinc (Zn) 0.0 - 0.30
Tin (Sn) 0.0 - 0.05
Chromium (Cr) 0.0 - 0.30
Titanium (Ti) 0.0 - 0.20
Other (Each) 0.0 - 0.05
Others (Total) 0.0 - 0.15
Aluminium (Al) Balance
Physical PropertyValue
Density 2.72 Kg/m³
Thermal Expansion 23.4 x10^-6 /K
Modulus of Elasticity 69 GPa
Thermal Conductivity 138 W/m.K
Electrical Resistivity 0.057 x10^-6 Ω .m
Mechanical PropertyValue
Proof Stress 330 Min MPa
Tensile Strength 360 Min MPa
Elongation 4 %
Hardness Brinell 95 Min HB

Aluminium alloy 6026 is a recent developed alloy meeting the following European Environmental Protection Directives:
# 2000/53/CE-ELV – For the automotive sector
# 2002/95/CE-RoHS – For the electrical and electronics sector

Alloy 6026 does not contain Tin (Sn) which can cause weakness and cracking of machined parts when subjected to stress and high temperature.
Alloy 6026 has excellent corrosion resistance and is suitable for anodising to provide both decorative and hard anodised finishes.

Alloy 6026 is a good alternative to alloys 6061 and 6082. Extruded Bars in alloy 6026 have the same minimum tensile strength as alloys 2011 & 2030.

Applications
6026 can be used in place of alloys 6082 or 6081, especially where the finished parts require extensive machining
~ Machined Parts – Especially on high speed automatic lathes
~ Decorative Anodising
~ Hard Anodising
~ Hot Forging
~ Automotive Components such as Brake Systems
~ Electrical & Electronic Parts

Temper Types

The most common temper for 6026 aluminium is:

  • T9 - Solution heat treated, artificially aged and cold worked

Supplied Forms

Alloy 6026 is typically supplied as extruded and/or drawn bar

  • Bar

Machinability

6026 can be used in place of alloys 6082 or 6081, especially where the finished parts require extensive machining on high speed automtatic lathes and machining centres

Weldability

Weldability of alloy 6026 is good 

This Data is indicative only and must not be seen as a substitute for the full specification from which it is drawn. In particular, the mechanical property requirements vary widely with temper, product and product dimensions. The information is based on our present knowledge and is given in good faith. However, no liability will be accepted by the Company is respect of any action taken by any third party in reliance thereon.

As the products detailed may be used for a wide variety of purposes and as the Company has no control over their use; the Company specifically excludes all conditions or warranties expressed or implied by statute or otherwise as to dimensions, properties and/or fitness for any particular purpose.

Any advice given by the Company to any third party is given for that party’s assistance only and without liability on the part of the Company. Any contract between the Company and a customer will be subject to the company’s Conditions of Sale. The extent of the Company’s liabilities to any customer is clearly set out in those Conditions; a copy of which is available on request.

Get Adobe Reader

Certain files on this page will require the Adobe Reader software. We recommend using the latest version if you don't already have it. Click on the "Get Adobe Reader" image to download the latest version now.